Link to full record for micrograph 606 Micrograph 606 : Extruded Saffil-containing metal matrix composite
System: Al, Composition: Commercial purity (99.5%)
Reflected light microscopy, polarised
40 μm
Link to full record for micrograph 610 Micrograph 610 : Section of a metal matrix composite (MMC)
System: Al, Composition: Commercial purity (99.5%) + 15 micron angular silicon carbide particles
Reflected light microscopy, polarised
40 μm
Link to full record for micrograph 611 Micrograph 611 : Section of a metal matrix composite (MMC) after extrusion and annealing
System: Al, Composition: Commercial purity (99.5%) + 13 micron alumina spheroids
Reflected light microscopy, polarised
40 μm
Link to full record for micrograph 616 Micrograph 616 : Cavity formation in a tensile loaded alumina particulate composite
System: Al, Composition: Commercial purity (99.5%) + 15 micron angular alumina particles
Scanning electron microscopy (SEM)
80 μm
Link to full record for micrograph 618 Micrograph 618 : Fracture surface of a carbon fibre composite
System: CCcomposite, Composition: Carbon fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
600 μm
Link to full record for micrograph 619 Micrograph 619 : Tensile failure surface of a carbon fibre composite
System: CCcomposite, Composition: Carbon fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
100 μm
Link to full record for micrograph 620 Micrograph 620 : Kevlar fibre composite fracture surface
System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
600 μm
Link to full record for micrograph 621 Micrograph 621 : Kevlar fibre composite shear surface
System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
100 μm
Link to full record for micrograph 622 Micrograph 622 : Kevlar fibre composite shear surface
System: Kevlar composite, Composition: Kevlar fibre, epoxy resin matrix
Scanning electron microscopy (SEM)
100 μm
Link to full record for micrograph 623 Micrograph 623 : Space-filling fire-resistant composite Barrikade (R)
System: Barrikade, Composition: Expanded vermiculite, cured in ZnO and mixed with binder
Photography (no microscope)
10 mm