Contributor
103 micrographs contributed by Prof T W Clyne, ordered by micrograph number.
Showing 91 - 100 of 103 micrographs | Page 1 .. 5 6 7 8 9 10 11 | Previous | Next |
Micrograph
604
:
Extruded aluminium System: Al, Composition: Commercial purity (99.5%) Reflected light microscopy, polarised 40 μm |
|
Micrograph
605
:
Fracture surface formed by hot tearing (solidification cracking) System: Al, Composition: Commercial purity (99.5%) Scanning electron microscopy (SEM) 40 μm |
|
Micrograph
606
:
Extruded Saffil-containing metal matrix composite System: Al, Composition: Commercial purity (99.5%) Reflected light microscopy, polarised 40 μm |
|
Micrograph
607
:
Fibre fracture in a metal matrix composite System: Al, Composition: Commercial purity (99.5%) Scanning electron microscopy (SEM) 4 μm |
|
Micrograph
608
:
Channelling contrast TEM image of subgrains of extruded aluminium System: Al, Composition: Commercial purity (99.5%) Transmission electron microscopy (TEM) 600 nm |
|
Micrograph
609
:
The grain structure of extruded aluminium System: Al, Composition: Commercial purity (99.5%) Reflected light microscopy, polarised 40 μm |
|
Micrograph
610
:
Section of a metal matrix composite (MMC) System: Al, Composition: Commercial purity (99.5%) + 15 micron angular silicon carbide particles Reflected light microscopy, polarised 40 μm |
|
Micrograph
611
:
Section of a metal matrix composite (MMC) after extrusion and annealing System: Al, Composition: Commercial purity (99.5%) + 13 micron alumina spheroids Reflected light microscopy, polarised 40 μm |
|
Micrograph
612
:
Nematic liquid crystalline polymer System: Liquid crystalline polymer, Composition: K24 (4-cyano-4'-8-alkylbiphenyl) Cross-polarised light microscopy 100 μm |
|
Micrograph
613
:
Facetted aluminium dendrites System: Al-Sn, Composition: Al 15, Sn 85 (wt%) Reflected light microscopy 80 μm |
Showing 91 - 100 of 103 micrographs | Page 1 .. 5 6 7 8 9 10 11 | Previous | Next |