Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Contributor
9 micrographs contributed by Prof A H Windle, ordered by micrograph number.
![]() |
Micrograph
561
:
Ordered film of carbon nanotubes System: Carbon nanotube, Composition: Not specified Field emission gun scanning electron microscopy (FEGSEM) 400 nm |
![]() |
Micrograph
562
:
Multi-walled carbon nanotube System: Carbon nanotube, Composition: Not specified Transmission electron microscopy (TEM) 3.2 nm |
![]() |
Micrograph
563
:
Carbon nanotubes System: Carbon nanotube, Composition: Low concentration (<0.3 vol%) suspension in water Field emission gun scanning electron microscopy (FEGSEM) 99 nm |
![]() |
Micrograph
637
:
Disclinations in a smectic LCP, revealed by decoration System: Liquid crystalline polymer, Composition: Semi-flexible LCP, Cl-7 Cross-polarised light microscopy 10 μm |
![]() |
Micrograph
638
:
Disclinations in a smectic LCP, revealed by decoration System: Liquid crystalline polymer, Composition: Semi-flexible LCP, Cl-8 Cross-polarised light microscopy 10 μm |
![]() |
Micrograph
639
:
Twist-escaped loops in the liquid crystalline polymer MBBA System: Liquid crystalline polymer, Composition: MBBA Cross-polarised light microscopy 200 μm |
![]() |
Micrograph
640
:
Fracture surface in a liquid crystalline polymer, oriented by a magnetic field System: Liquid crystalline polymer, Composition: Random copolyester of average molecular weight 14401 Scanning electron microscopy (SEM) 4 μm |
![]() |
Micrograph
641
:
Fracture surface in a liquid crystalline polymer System: Liquid crystalline polymer, Composition: Random copolyester of average molecular weight 14401 Scanning electron microscopy (SEM) 12 μm |
![]() |
Micrograph
642
:
Fracture surface in a liquid crystalline polymer System: Liquid crystalline polymer, Composition: Random copolyester of average molecular weight 14402 Scanning electron microscopy (SEM) 12 μm |