Micrograph 545 and full record
- Micrograph no
- 545
- Brief description
- Fibre reinforced magnesium aluminosilicate ceramic showing black areas of porosity
- Keywords
- ceramic
, fibre
, magnesium aluminosilicate, porosity 
- Categories
- Ceramic
- System
- SiC fibre-reinforced magnesium aluminosilicate
- Composition
- Not specified
- Standard codes
- Reaction
- Processing
- The fibres are drawn and infiltrated with a slurry consisting of a powdered matrix in an organic binder and water.. The mixture is hot pressed to give a dense composite.
- Applications
- Sample preparation
- Polished
- Technique
- Reflected light microscopy
- Length bar
- 100 μm
- Further information
- Contributor
- Dr K M Knowles
- Organisation
- Department of Materials Science and Metallurgy, University of Cambridge
- Date
- 01/10/02
- Licence for re-use
Attribution-NonCommercial-ShareAlike 4.0 International- Related micrographs
- Micrograph 548: Fractograph showing extensive matrix cracking and fibres bridging an opened matrix in a fibre reinforced magnesium aluminosilicate ceramic (200 μm)
- Micrograph 550: Micrograph showing the complex chemical reactions which arise at fibre-matrix interfaces in a fibre reinforced magnesium aluminosilicate ceramic subjected to oxidation (300 nm)
View image alone .. in a new window