Video Library
Browse the libraryAdvanced searchHelpAbout the video libraryTerms of useFeedback Print this page

Category
85 videos for category Experimental procedure:
| Showing 41 - 50 of 85 videos | Page 1 2 3 4 5 6 7 8 9 | Previous | Next |
Image
![]() |
video 60 : Video demonstrating that the stiffness of rubber is proportional to temperature. The rubber is extended under a fixed load, and contracts when heated due to the increased stiffness, and therefore reduced strain. From TLP: The Stiffness of Rubber |
Image
![]() |
video 61 : Single crystal X-ray diffractometer experiment with lithium fluoride crystal showing the first diffraction peak at the first Bragg angle. From TLP X-ray diffraction techniques |
Image
![]() |
video 62 : Single crystal X-ray diffractometer experiment with lithium fluoride crystal showing the second diffraction peak at the second Bragg angle. From TLP X-ray diffraction techniques |
Image
![]() |
video 71 : Impact testing of a polymer specimen. |
Image
![]() |
video 77 : A coil of solder creeping under its own weight at 28 °C. From TLP Creep deformation of metals |
Image
![]() |
video 78 : A coil of solder creeping under its own weight at 65 °C. From TLP Creep deformation of metals |
Image
![]() |
video 79 : A coil of solder creeping under its own weight at 85 °?C. From TLP Creep deformation of metals |
Image
![]() |
video 80 : Heating a PET bottle over a bunsen burner flame. Before heating the plastic is in a less crystalline state than would be expected, as a result of the production process. Upon heating it recrystallises into a denser form, and therefore shrinks. (related topic - recycling polymers) |
Image
![]() |
video 81 : A three-point bend test to measure the deflection and failure load of a greenheart wood sample. From TLP The Structure and Mechanical Behaviour of Wood |
Image
![]() |
video 82 : A three-point bend test to measure the deflection of a scotspine sample. From TLP The Structure and Mechanical Behaviour of Wood |
| Showing 41 - 50 of 85 videos | Page 1 2 3 4 5 6 7 8 9 | Previous | Next |