Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Micrograph 550 and full record
- Micrograph no
- 550
- Brief description
- Micrograph showing the complex chemical reactions which arise at fibre-matrix interfaces in a fibre reinforced magnesium aluminosilicate ceramic subjected to oxidation
- Keywords
- ceramic
, fibre
, magnesium aluminosilicate - Categories
- Ceramic
- System
- SiC fibre-reinforced magnesium aluminosilicate
- Composition
- Not specified
- Standard codes
- Reaction
- Processing
- The fibres are drawn and infiltrated with a slurry consisting of a powdered matrix in an organic binder and water.. The mixture is hot pressed to give a dense composite.
- Applications
- Sample preparation
- Technique
- Bright-field TEM
- Length bar
- 300 nm
- Further information
- An approximately 1.2 micrometre thick interfacial region is seen between the matrix and the fibre. I1-4 are four distinct interlayers with different compositions within this region.
- Contributor
- Dr K M Knowles
- Organisation
- Department of Materials Science and Metallurgy, University of Cambridge
- Date
- 01/10/02
- Licence for re-use
Attribution-NonCommercial-ShareAlike 4.0 International- Related micrographs
View image alone .. in a new window
Help is available on downloading images