Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Micrograph 629 and full record
- Micrograph no
- 629
- Brief description
- FORMGRIP closed cell aluminium foam
- Keywords
- alloy
, aluminium
, aluminium foam, cell
, composite foam, composite material
, foam
, FORMGRIP, metal - Categories
- Foam, Metal or alloy, Metal or alloy composite foam
- System
- Al
- Composition
- Not specified
- Standard codes
- Reaction
- Pre-oxidised titanium hydride is used as a foaming agent
- Processing
- The FORMGRIP technique involves use of 1 to 3 wt% titanium hydride to a modified melt as a foaming agent
- Applications
- Closed cell aluminium foams are an ultra-light material, with potential structural applications in transport and construction. They may also be used in energy absorbing structures and heat exchangers
- Sample preparation
- Technique
- Photography (no microscope)
- Length bar
- 6 mm
- Further information
- Additions such as SiC are made to molten aluminium or aluminium alloy to modify the melt viscosity and make it suitable for foaming. 1 to 3 wt% of pre-oxidised titanium hydride is then added to the melt which is solidified to form a precursor which can be foamed in a controlled manner by a subsequent heat treatment. The resulting foam has a relatively fine and uniform cell structure.
- Contributor
- Dr V Gergely
- Organisation
- Department of Materials Science and Metallurgy, University of Cambridge
- Date
- 03/10/02
- Licence for re-use
Attribution-NonCommercial-ShareAlike 4.0 International- Related micrographs
View image alone .. in a new window
Help is available on downloading images