Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Micrograph 640 and full record
- Micrograph no
- 640
- Brief description
- Fracture surface in a liquid crystalline polymer, oriented by a magnetic field
- Keywords
- alignment, fibre
, fibrillation
, fracture
, liquid crystalline polymer (LCP), lyotropic, magnetic, nematic, polymer 
- Categories
- Fracture, Polymer
- System
- Liquid crystalline polymer
- Composition
- Random copolyester of average molecular weight 14401
- Standard codes
- Reaction
- Processing
- A 1.1T magnetic field has been applied for one hour (magnetic axis vertical)
- Applications
- The molecules in a LCP mesophase can be steered by external fields; a property used in display technology. Alignment is also exploited in high strength fibres like Kevlar and mouldable Vectra
- Sample preparation
- Technique
- Scanning electron microscopy (SEM)
- Length bar
- 4 μm
- Further information
- Above their melting point, liquid crystalline polymers exhibit a mesophase within which, although able to flow and are not arranged in a crystal, they exhibit long range orientational order. This molecular alignment can be exploited to make high strength and stiffness fibres such as Kevlar, or even mouldable thermotropics such as Vectra. Molecular alignment can also be controlled by an external applied field; a property exploited in liquid crystal displays. This polymer has been subjected to a magnetic field of 1.1T (normal to the fracture plane) for one hour and the resulting alignment is evident in the fractured surface.
- Contributor
- Prof A H Windle
- Organisation
- Department of Materials Science and Metallurgy, University of Cambridge
- Date
- 03/10/02
- Licence for re-use
Attribution-NonCommercial-ShareAlike 4.0 International- Related micrographs
View image alone .. in a new window
Help is available on downloading images