DoITPoMS Micrograph Library Micrograph 756 and full record

Micrograph 756 and full record

Link to image file for micrograph 756
Micrograph no
756
Brief description
Bi 50, Sn 50 (wt%)
Keywords
alloy Link to MATTER Glossary entry for alloy, bismuth, metal, tin
Categories
Metal or alloy
System
Bi-Sn   Link to phase diagram
Composition
Bi 50, Sn 50 (wt%)
Standard codes
Reaction
Processing
Small casting in alumina crucible - air cooled.
Applications
Educational alloy - low melting point allows easy and safe use for students.
Sample preparation
Standard polishing techniques.
Technique
Scanning electron microscopy (SEM) in secondary electron imaging (SEI) mode
Length bar
300 μm
Further information
A coarse dendritic structure can be clearly seen, with no clear preferred orientation.
Contributor
M Charles and A Cockburn
Organisation
Department of Materials Science and Metallurgy, University of Cambridge
Date
07/05/03
Licence for re-use
Attribution-Non-Commercial-Share Alike 2.0 UK: England & Wales
Related micrographs

View image alone .. in a new window

View micrograph only

View full record only

Help is available on downloading images